Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.1 µm/m-°C @Temperature 37.8 - 538 °C |
6.75 µin/in-°F @Temperature 100 - 1000 °F |
|
Meehanite AQ Flake Graphite Cast Iron Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate.. |