Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 112 µm/m-°C | 62.4 µin/in-°F | Perpendicular to Laminate |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
CTE, linear | 112 µm/m-°C | 62.4 µin/in-°F | Perpendicular to Laminates |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |