Thermal Properties Metric English Comments
CTE, linear 13.24 µm/m-°C

@Temperature 0.000 - 20.0 °C
7.356 µin/in-°F

@Temperature 32.0 - 68.0 °F
Mateck Quartz Crystalline (SiO2)
Optical crystals