Polymer Property : CTE, linear = 7.361 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 13.25 µm/m-°C

@Temperature 24.0 - 204 °C
7.361 µin/in-°F

@Temperature 75.2 - 399 °F
Latrobe Graph-Air® Cold Work Tool Steel (ASTM A10)
Graph-Air tool steel is an air-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles w..