Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 50.0 - 70.2 µm/m-°C | 27.8 - 39.0 µin/in-°F | Average value: 65.5 µm/m-°C Grade Count:29 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
CTE, linear | 56.0 - 70.2 µm/m-°C | 31.1 - 39.0 µin/in-°F | Average value: 66.5 µm/m-°C Grade Count:19 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |