Thermal Properties Metric English Comments
CTE, linear 702 µm/m-°C

@Temperature 20.0 °C
390 µin/in-°F

@Temperature 68.0 °F
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin..