Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.7 µm/m-°C | 42.1 µin/in-°F | Below Tg |
Tra-Con Tra-Bond F113SC High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC is a room temperature curing, high Tg and low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors. It has also been used for bonding LED displays, lense.. |