Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 79.6 µm/m-°C @Temperature 20.0 °C |
44.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Shuman 810 Black Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
CTE, linear | 79.6 µm/m-°C @Temperature 20.0 °C |
44.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Shuman 880 Grey Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
CTE, linear | 79.6 µm/m-°C | 44.2 µin/in-°F | ASTM D696 |
Shuman SP810 Black Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
CTE, linear | 79.6 µm/m-°C | 44.2 µin/in-°F | ASTM D696 |
Shuman SP880 Grey Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |