Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.6 µm/m-°C | 8.10 µin/in-°F | |
Weartech International WT-32 Cobalt Hardfacing & Wear Resistant Alloy Applications: engine valves and seatsInformation provided by Weartech International |
|||
CTE, linear | 14.6 µm/m-°C | 8.10 µin/in-°F | |
Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy Applications: pump sleevesInformation provided by Weartech International |