Thermal Properties Metric English Comments
CTE, linear 8.15 µm/m-°C

@Temperature 260 °C
4.53 µin/in-°F

@Temperature 500 °F
Ferro EG 4000 Display Device
Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and ..
CTE, linear 8.15 µm/m-°C

@Temperature 260 °C
4.53 µin/in-°F

@Temperature 500 °F
Ferro EG 4010 Display Device
Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas..