CTE, linear 85.5 µm/m-°C
47.5 µin/in-°F
Hexcel® HexPly® F185 Epoxy Resin
HexPly® F185 is an advanced epoxy formulation designed for autoclave curing to offer very high sandwich and metal bonding strengths with moderate laminate strengths. HexPly® F185 is a structural a..