Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 155 µm/m-°C @Temperature 20.0 °C |
86.1 µin/in-°F @Temperature 68.0 °F |
|
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to.. |
|||
CTE, linear | 155 µm/m-°C @Temperature 20.0 °C |
86.1 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Spartech Royalite R59M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in t.. |
|||
CTE, linear | 155 µm/m-°C @Temperature 20.0 °C |
86.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |