Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 9.36 µm/m-°C

@Temperature 20.0 °C
5.20 µin/in-°F

@Temperature 68.0 °F
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic
High dielectric and mechanical strength. For high voltage insulators, lamp housings, thermal switches, and radiation parts. Readily machined, no firing required. Plates from 1/8" to 1" thick; rod..