Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 50.0 - 91.0 µm/m-°C | 27.8 - 50.6 µin/in-°F | Average value: 81.3 µm/m-°C Grade Count:46 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |