Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 176 µm/m-°C | 97.8 µin/in-°F | T>Tg; 90 Minute UV Cure; SLA 3500 System; ASTM E831-93 |
3D Systems Accura® accuGen™ Nd Plastic for SLA® Systems Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® Viper si2™, 3500, 5000 & 7000 systems.Typical ApplicationsMulti-purpose mode.. |