Glass Transition Temp, Tg 172 °C

@Thickness <=0.0508 mm
342 °F

@Thickness <=0.00200 in
TMA; ASTM D3850
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material
SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a ..