Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | <= 0.0210 W/m-K | <= 0.146 BTU-in/hr-ft²-°F | normal ambient conditions; ASTM C518, ISO 8301 |
Microtherm Group SlimVac Filament Reinforced Silica Vacuum Insulation Panel Microtherm® SlimVac panels are high performance evacuated microporous insulation panels covered in an impermeable outer envelope. The insulation is an opacified blend of filament reinforced silic.. |