Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0420 W/m-K | 0.291 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0420 W/m-K | 0.291 BTU-in/hr-ft²-°F | mean temp of 80°C; ISO 8301 |
Zotefoams ZOTEK® N B50 High Performance Nylon Foam Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0420 W/m-K | 0.291 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |