Polymer Property : Thermal Conductivity = 0.0663 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0663 W/m-K
0.460 BTU-in/hr-ft²-°F
ASTM C177
Ensinger Tecapeek® XP-110 Compression Molded PEEK Compound, 45% Mineral Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..