Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0680 W/m-K @Temperature -40.0 °C |
0.472 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
|
3M Novec™ 774 Engineered Fluid 3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high.. |