Thermal Conductivity 0.0793 W/m-K
0.550 BTU-in/hr-ft²-°F
ASTM C-518
Saint-Gobain T-Bond II® Semi-Rigid Polyurethane Foam Structural Glazing and Cladding Spacer System
Description: Semi-Rigid Polyurethane Foam Substrate used as a Structural Glazing and Cladding Spacer System for In-Shop Fabrication. Semi-Rigid Polyurethane: An open cell structure allows air and mo..