Thermal Properties Metric English Comments
Thermal Conductivity 0.0860 W/m-K
0.597 BTU-in/hr-ft²-°F
ASTM C158
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..