Thermal Properties Metric English Comments
Thermal Conductivity 0.0950 W/m-K

@Temperature 100 °C
0.659 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM D1530
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..