Polymer Property : Thermal Conductivity = 0.181 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.181 W/m-K
1.26 BTU-in/hr-ft²-°F
Dow AIM® 4800 High Impact Styrenic Resin
AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..
Thermal Conductivity 0.181 W/m-K
1.26 BTU-in/hr-ft²-°F
Dow AIM® 4810 High Impact Styrenic Resin
AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..