Polymer Property : Thermal Conductivity = 0.207 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.207 W/m-K
1.44 BTU-in/hr-ft²-°F
Styron CALIBREâ„¢ 300EP 22 Polycarbonate, General Purpose
CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p..
Thermal Conductivity 0.207 W/m-K
1.44 BTU-in/hr-ft²-°F
Styron Pulse® B250 ABS + Polycarbonate
PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. ..