Polymer Property : Thermal Conductivity = 0.214 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.173 - 0.214 W/m-K
1.20 - 1.49 BTU-in/hr-ft²-°F
Average value: 0.187 W/m-K Grade Count:12
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..