Polymer Property : Thermal Conductivity = 0.285 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9035 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9255 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9280 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9235 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9270 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea..
Thermal Conductivity 0.0410 W/m-K
0.285 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9435 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..