Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 - 0.290 W/m-K | 1.60 - 2.01 BTU-in/hr-ft²-°F | Average value: 0.263 W/m-K Grade Count:6 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |