Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0450 W/m-K | 0.312 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0450 W/m-K | 0.312 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9270 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0450 W/m-K | 0.312 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9280 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |