Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.335 - 0.377 W/m-K | 2.32 - 2.61 BTU-in/hr-ft²-°F | |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |