Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.4068 W/m-K | 2.818 BTU-in/hr-ft²-°F | ASTM C177 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Thermal Conductivity | 0.4068 W/m-K | 2.818 BTU-in/hr-ft²-°F | ASTM C177 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |