Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | <= 0.465 W/m-K @Temperature 500 °C |
<= 3.23 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics REFINSUL ZAP-019 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Thermal Conductivity | 0.465 W/m-K @Temperature 500 °C |
3.23 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Thermal Conductivity | 0.465 W/m-K | 3.23 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 13LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |