Polymer Property : Thermal Conductivity = 0.530 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.490 - 0.530 W/m-K

@Temperature 40.0 - 40.0 °C
3.40 - 3.68 BTU-in/hr-ft²-°F

@Temperature 104 - 104 °F
Average value: 0.510 W/m-K Grade Count:2
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..