Thermal Properties Metric English Comments
Thermal Conductivity 0.988 W/m-K
6.86 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.988 W/m-K
6.86 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.988 W/m-K
6.86 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.988 W/m-K
6.86 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..