Polymer Property : Thermal Conductivity = 1.05 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.850 - 1.05 W/m-K
5.90 - 7.29 BTU-in/hr-ft²-°F
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported
Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In..