Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.168 W/m-K | 1.17 BTU-in/hr-ft²-°F | |
Americas Styrenics Styron® 6010 High Impact Polystyrene
(discontinued **) STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac.. |
|||
Thermal Conductivity | 0.169 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1700 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Thermal Conductivity | 0.169 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® DP 1-9349/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Thermal Conductivity | 0.168 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 1943 is a type 6 nylon graft copolymer developed for injection molding applications requiring improved dry as molded toughness, and increased flexibility. It has an excellent thermal and che.. |
|||
Thermal Conductivity | 0.169 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.169 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Thermal Conductivity | 0.169 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.168 W/m-K | 1.17 BTU-in/hr-ft²-°F | Melt |
BASF Capron® BG50XFI Impact Modified Nylon 6 (Dry)
(discontinued **) Capron BG50XFI is an injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths. It is also available in natura.. |