Polymer Property : Thermal Conductivity = 1.20 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 - 1.20 W/m-K
7.63 - 8.33 BTU-in/hr-ft²-°F
Average value: 1.13 W/m-K Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..