Polymer Property : Thermal Conductivity = 1.65 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.238 W/m-K
1.65 BTU-in/hr-ft²-°F
ASTM D-2863
Saint-Gobain Norton® ETFE Fluoropolymer Film
Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th..