Polymer Property : Thermal Conductivity = 1.74 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.74 W/m-K

@Temperature 600 °C
12.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Hot Face
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..