Polymer Property : Thermal Conductivity = 1.87 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.250 - 0.270 W/m-K
1.74 - 1.87 BTU-in/hr-ft²-°F
Average value: 0.258 W/m-K Grade Count:5
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Thermal Conductivity 0.159 - 0.270 W/m-K
1.10 - 1.87 BTU-in/hr-ft²-°F
Average value: 0.211 W/m-K Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..