Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 145 - 230 W/m-K | 1010 - 1600 BTU-in/hr-ft²-°F | |
H.C. Starck WCu 75/25 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
Thermal Conductivity | 145 W/m-K | 1010 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® 30W3 Infiltrated Copper Tungsten contact material ASTM B702, Class E, infiltrated, RWMA Class 12 For projection welding dies, die facing, and resistance welding electrodes. Also used for low expansion structural members. Information provided by CMW Inc. |