Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 7026 Copper Nickel, 1/2 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 7026 Copper Nickel, 1/4 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 7026 Copper Nickel, Annealed 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 70265 XP175, 1/2 Hard Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 70265 XP175, 1/4 Hard Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 70265 XP175, 3/4 Hard Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 70265 XP175, Annealed Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F | |
Eagle Brass 70265 XP175, Hard Information provided by Eagle Brass Company |
|||
Thermal Conductivity | 15.5 - 16.5 W/m-K | 108 - 115 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories Shelf Boards and Pillars SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |