Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.44 - 1.59 W/m-K | 10.0 - 11.0 BTU-in/hr-ft²-°F | |
Master Bond Super Gel 9AOND Dimensionally Stable Urethane Modified Epoxy Master Bond Super Gel 9AOND is a two component, urethane modified epoxy system that cures at room temperature and has a paste-like consistency. It offers softness and retains dimensional stability. .. |