Thermal Properties Metric English Comments
Thermal Conductivity 110 W/m-K
763 BTU-in/hr-ft²-°F
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite
Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif..
Thermal Conductivity 110 W/m-K
763 BTU-in/hr-ft²-°F
Cytec Thornel® P-55S 4K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla..
Thermal Conductivity 110 W/m-K
763 BTU-in/hr-ft²-°F
Cytec Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Thermal Conductivity 110 W/m-K
763 BTU-in/hr-ft²-°F
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.