Thermal Conductivity 17.2 W/m-K

@Temperature 100 °C
119 BTU-in/hr-ft²-°F

@Temperature 212 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..