Polymer Property : Thermal Conductivity = 123 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 123 W/m-K
852 BTU-in/hr-ft²-°F
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals