Polymer Property : Thermal Conductivity = 129 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 18.6 W/m-K

@Temperature 500 °C
129 BTU-in/hr-ft²-°F

@Temperature 932 °F
Perpendicular
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..