Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 198 W/m-K | 1370 BTU-in/hr-ft²-°F | |
Goodfellow Copelmet® Tungsten 72/Copper 28 Alloy Developed as an electrode material, this alloy is used for spark erosion electrodes and contacts giving excellent resistance to mechanical wear and electrical erosion.Information provided by Goodfel.. |
|||
Thermal Conductivity | 197 W/m-K | 1370 BTU-in/hr-ft²-°F | Drawn rod, bar and strip |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Thermal Conductivity | 197 W/m-K | 1370 BTU-in/hr-ft²-°F | Forging |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |