Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.04 W/m-K | 14.2 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-175 is a two component epoxy designed for semiconductor die-attach. It is a higher Tg version of EPO-TEK® H20E. It was designed to be used in semiconductor / J.. |