Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.288 - 22.0 W/m-K | 2.00 - 153 BTU-in/hr-ft²-°F | Average value: 5.71 W/m-K Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |